Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Physics of nail pullout 1

Status
Not open for further replies.

crossframe

Structural
Mar 30, 2004
276
I'm curious as to the mechanics that causes nails to back out of wood. I understand that normal moisture and drying cycles can cause nails to back out of the holes, but I'm talking about nails that end up an inch or more out of the wood - far beyond the "swollen" size of wet wood - and can easily be removed by hand. Is it lateral squeezing on the small tapered nail-tip? Vibration?
 
Replies continue below

Recommended for you

It's ratcheting. Each time the wood swells it pushes the nail out a little, then it shrinks, grabs it again and pushes with the next swell.

Engineering is the art of not constructing...of doing that well with one dollar what any bungler can do well with two after a fashion.
 