Pile Cut-offs at an angle 1

Status
Not open for further replies.

Dinosaur

Structural
Mar 14, 2002
538
I am looking for a spec that calls for piles or other posts to be cut off at an angle to help prevent rainwater from penetrating the end grain. The railroad industry once did this when the original telegraph lines were installed, but I don't know where to go now for an example. I have proposed this in our highway construction specs and have been asked to substantiate it. Common sense is not adequate justification to many. Thx
 
Replies continue below

Recommended for you

I would protect the ends of the piles rather than cut them at an angle to promote run-off.

Under normal conditions, I would not permit piles to be cut off at an angle.

Dik
 
I guess I was not clear.

If you were going to install a sign supported by a wood post, would you think it unwise to cut the top of the post at an angle to prevent rainwater from attacking the top of the post?
 