Hclrag123
Mechanical
- Dec 29, 2011
- 29
I am working on building a test fixture in the Pipe shape to withstand 3Million POunds of bending force.
The Pipe diameter can be anything between 56 to 60" O.D and wall thickness 1.25" (or more)and 40FT Long. The Yield and Tensile requirement is above 120KSi. Since it is practically impossible for us to procure a single Piece of pipe of X100/X120, i am thinking of getting plates rolled into pipes. In this regard, i have below questions.
1.Can we roll Weldox plates 1.25" Thk to a 60" O.D (or 56" O.D X 1.5" THK)pipe? If yes, can you please provide the contacts of those who can do this?
If no, what is the max thk that can be rolled?
2. Should this is be a cold rolled or hot rolled?
3. IF we roll FOur 10FT sections and weld them together will the strength be equal to the actual single pipe i.e can it with stand a bendng force of 3 Million Pounds? What kind of Welds should be good?
4. Is there any other material which has 120KSi or more tensile and yield, which can be eaily Rolled & Welded, easily procured within united states?
Thanks in advance.
The Pipe diameter can be anything between 56 to 60" O.D and wall thickness 1.25" (or more)and 40FT Long. The Yield and Tensile requirement is above 120KSi. Since it is practically impossible for us to procure a single Piece of pipe of X100/X120, i am thinking of getting plates rolled into pipes. In this regard, i have below questions.
1.Can we roll Weldox plates 1.25" Thk to a 60" O.D (or 56" O.D X 1.5" THK)pipe? If yes, can you please provide the contacts of those who can do this?
If no, what is the max thk that can be rolled?
2. Should this is be a cold rolled or hot rolled?
3. IF we roll FOur 10FT sections and weld them together will the strength be equal to the actual single pipe i.e can it with stand a bendng force of 3 Million Pounds? What kind of Welds should be good?
4. Is there any other material which has 120KSi or more tensile and yield, which can be eaily Rolled & Welded, easily procured within united states?
Thanks in advance.