Hello,
Finishing a CML&C steel pipeline design for the conveyance of raw water... Looking for a good reference or design manual which explicitly discusses the quantity and location of permanent reference electrodes. Our pipeline is about 5,000 feet in length and varies from 30 to 20 inches in diameter. The best I reference I've found thus far, by the US Bureau of Reclamation (Technical Memorandum No. MERL-2012-40) recommends the following:
1. At the each end of any electrically continuous pipeline.
2. Approximately every 1,000 feet for long electrically continuous segments of pipeline.
3. At one end of all casings.
4. At all foreign pipeline crossings.
5. At all sets of bonded metallic fittings on nonmetallic pipe.
6. At all bonded structures(buried yard metalwork, tanks, ect.)
7. As close to structure as possible.
8. Located to make them readily accessible.
9. Where test stations will not interfere with operations.
Are these recommendations sufficient? Or should I continue the search?
Thank you
Finishing a CML&C steel pipeline design for the conveyance of raw water... Looking for a good reference or design manual which explicitly discusses the quantity and location of permanent reference electrodes. Our pipeline is about 5,000 feet in length and varies from 30 to 20 inches in diameter. The best I reference I've found thus far, by the US Bureau of Reclamation (Technical Memorandum No. MERL-2012-40) recommends the following:
1. At the each end of any electrically continuous pipeline.
2. Approximately every 1,000 feet for long electrically continuous segments of pipeline.
3. At one end of all casings.
4. At all foreign pipeline crossings.
5. At all sets of bonded metallic fittings on nonmetallic pipe.
6. At all bonded structures(buried yard metalwork, tanks, ect.)
7. As close to structure as possible.
8. Located to make them readily accessible.
9. Where test stations will not interfere with operations.
Are these recommendations sufficient? Or should I continue the search?