ryuchangmyong
Mechanical
- Jul 30, 2014
- 33
Dear All
Currently, we are now in a pre-commissioning test for Demi-water piping at Power Plant alongwith 8 bar operation pressure of Demi-water pump (Transfering water from Demi-Tank), this piping include restruction orifice at the middle of recirculation pipe from discharging to Demi-Tank, Globe valve and Cone type filter also installed at Dicharge line, However, especially too much noise and vibration occurs at Discharge. Currently I guess that the problems is due to thin pipe line even though required thickness in accordance with ASME B31.1 satisfied.
1) Suction line : A312-TP304, 10" SCH. 10S (Thk 4.19mm)
2) Discharge line : A312-TP304, 8" SCH. 10S (Thk 3.76mm)
3) Recirculation line : A312-TP304, 6" SCH. 10S (Thk 3.4mm)
At first, we guessed that Restruction size and Location occurs noise, so, we have tried and changed orifice hole size and installed Dual orifice, finally we tried to install with Multiple hole type in order to reduce Dynamic flow force through Orifice, However, nothing could we shooting this problems.
So, I strongly believe that thin pipe thickness occurs this noise because in suction line, cosidering NPSHa of 0.5 Bar, there is no expected Pump cavitation or surging, hammering. (See Attached Piping Photo)
Could you have any similar experience such as this kind of trouble.
Currently, we are now in a pre-commissioning test for Demi-water piping at Power Plant alongwith 8 bar operation pressure of Demi-water pump (Transfering water from Demi-Tank), this piping include restruction orifice at the middle of recirculation pipe from discharging to Demi-Tank, Globe valve and Cone type filter also installed at Dicharge line, However, especially too much noise and vibration occurs at Discharge. Currently I guess that the problems is due to thin pipe line even though required thickness in accordance with ASME B31.1 satisfied.
1) Suction line : A312-TP304, 10" SCH. 10S (Thk 4.19mm)
2) Discharge line : A312-TP304, 8" SCH. 10S (Thk 3.76mm)
3) Recirculation line : A312-TP304, 6" SCH. 10S (Thk 3.4mm)
At first, we guessed that Restruction size and Location occurs noise, so, we have tried and changed orifice hole size and installed Dual orifice, finally we tried to install with Multiple hole type in order to reduce Dynamic flow force through Orifice, However, nothing could we shooting this problems.
So, I strongly believe that thin pipe thickness occurs this noise because in suction line, cosidering NPSHa of 0.5 Bar, there is no expected Pump cavitation or surging, hammering. (See Attached Piping Photo)
Could you have any similar experience such as this kind of trouble.