A company ordered a substantial quantity of 8" to 16" double random sch 40 A106B with beveled ends for tankfield piping. About half came in with the ends not cut square, more than 1/8" off. The piping contractor wants a substantial extra per pipe end, the pipe supplier says the A106B spec is silent on the end cut, the owner is feeling that one or both are failing them in that no one mentioned this in their quotation, no one is to blame and their bank account is taking a substantial hit.