I have been given conflicting information on the time that Duplex may be resistant to pitting: one source says 7 days, and the other several months.
My pipes may be exposed to some seawater content for 2 to 3 months (most of the content will be treated with oxygen scavengers, but the distribution cannot be guarenteed).
My valve body is carbon steel and will need CP and so isolation from the CP system would be imposible, ruling out super Duplex.
If the 7 days is correct then I need to find another material solution, but if I can resist pitting for a couple of months then Duplex will be suitable.