Does anyone have experience with no-fines concrete when tremie placed underwater? We have a situation where the owner (the State) would like to fill the void between a new bulkhead and an old bulkhead with concrete. We are worried about large differential water levels if the void was filled with traditional concrete. Are there issues with maintaining the drainage function of the no-fines concrete when tremie placed under water?