Dear,
I am doing suspension polymerization of methyl methacrylate
BPO-DMPT is used as initiator at room temp (~5.5wt % of monomer)
PVA (I tried 99% and 88% hydrolized) as suspending agent (1wt% of water)
monomer:water : 1:3.6
I fail to obtain the bead but an aggregated mass for 99% PVA and soft clumps for 88% PVA
Please advice how to overcome this and obtain PMMA in beads.
Thank you for your time
Best regards