Polymers vs elastomers? 1

Status
Not open for further replies.

321GO

Automotive
Jan 24, 2010
345
Hi guys, hope you're all well.

What is the difference between the term "ploymers" and "elastomers"?

I'm somewhat confused?

[love]
 
Replies continue below

Recommended for you

Polymers are materials composed of many repeating units. The final polymer can be thermoplastic, thermosetting, or elastomeric. An elastomer has low elastic modulus and large elastic strain. Rubber would be a type of elastomer, nylon is a thermoplastic and epoxy is a thermoset.
 
Polymers and elastomers are both, in essence, the same thing. They are made of long chain molecules. In the case of elastomers those molecules are very flexible at room temperature. In the case of polymers they are quite rigid at room temperature.

Chris DeArmitt PhD
President - Phantom Plastics LLC

Consulting, ideas and training on plastic materials
 