Mechanical
- Mar 14, 2003
- 3
A machined plastic part designed and sourced in England lists the material as "thermally stabilized polypropylene". It has a smooth finish and an opaque biege/gray color. I want to make some parts from the same material, but I can not get a detailed spec from the UK supplier, and I can not find a source for this kind of polypropylene in the US. Supposedly, this material is common in the UK.
I got a sample of Propylux HS from Westlake Plastics. It is heat stabilized, but it is a bright white color and so does not match the beige/gray parts from the UK.
Any ideas how to identify and locate a source for this plastic?
I got a sample of Propylux HS from Westlake Plastics. It is heat stabilized, but it is a bright white color and so does not match the beige/gray parts from the UK.
Any ideas how to identify and locate a source for this plastic?