rachnatbovo
Mechanical
thread794-437308
Hi Sirs,
Similar topic I have seen as below link: I still a bit unsure the below:
The Head End was cold formed from the plate super DSS( SA 240 32750) 10H, nominal thick 8mm(min req 6.8mm), Fiber elongation was calculated is 3.5% ( The vessel is designed for Lethal service (H2S) as refer to the DS & GA drawing).
-> Client has a comment to require annealing solution shall be performed after forming!!!
However, I understand that postforming heat treatment (Annealing solution) is not necessary for Duplex and Super Duplex with two phases given their potential to form deleterious intermetallic phases at temperatures below the solution annealing temperature, also affect to corrosion resistance of material....etc
ASME Sec VIII Div1 does not required nor recommended annealing solution for grade 10H,
So, I would appreciate if someone could shed some more light on this topic, then I should arise an concession request to avoid risk in this case.
Thank you very much
Hi Sirs,
Similar topic I have seen as below link: I still a bit unsure the below:
The Head End was cold formed from the plate super DSS( SA 240 32750) 10H, nominal thick 8mm(min req 6.8mm), Fiber elongation was calculated is 3.5% ( The vessel is designed for Lethal service (H2S) as refer to the DS & GA drawing).
-> Client has a comment to require annealing solution shall be performed after forming!!!
However, I understand that postforming heat treatment (Annealing solution) is not necessary for Duplex and Super Duplex with two phases given their potential to form deleterious intermetallic phases at temperatures below the solution annealing temperature, also affect to corrosion resistance of material....etc
ASME Sec VIII Div1 does not required nor recommended annealing solution for grade 10H,
So, I would appreciate if someone could shed some more light on this topic, then I should arise an concession request to avoid risk in this case.
Thank you very much