SkyPunk
Aerospace
- Jul 4, 2006
- 12
Anyone have a quick sumation of what possible effects could be expected of the following. Aluminum forging shot peened with 200% coverage damaged appx .006 deep gouge appx 1" long .008" wide. Damaged area blended out 10/1(ish), and shot peen not replaced? Most allowables of surface material are 10% of shot peen intensity. This particular one works out to allow .001" material removal allowable. How severe, if any would the reduction in fatigue life be?
Thanks,
Skypunk
Thanks,
Skypunk