Aesur
Structural
- Jun 25, 2019
- 855
I am curious if someone could explain to me why with PT slabs on grade the deflection limits for "Prefab Roof Trusses spanning the full length or width of the foundation" are limited to L/1000 for Center Lift and L/2000 for Edge Lift. Wouldn't this apply to most residential structures? In my experience it is common for most engineers in the Southwest US to design the PT slabs for L/240 and L/480 (Wood Frame), even when the structures typically have Stucco or Plaster walls (L/360 and L/720).