Hello, I have the following question.
We have welded a trunnion to a pipe with a full penetration single side weld. This weld, because of the thickness of the trunnion (65mm), has required PWHT as specification requires PWHT for thickness over 40mm. After being treated, a modification of the dwg requires a fillet weld with a leg of 45mm. As per specification this fillet weld would require PWHT.
I would like to know if the requirement of PWHT can be avoided, as they have already qualified a CJP WPS without PWHT, that would cover up to 40mm (over 40mm would require PWHT), and this would cover all fillet welds.
We have welded a trunnion to a pipe with a full penetration single side weld. This weld, because of the thickness of the trunnion (65mm), has required PWHT as specification requires PWHT for thickness over 40mm. After being treated, a modification of the dwg requires a fillet weld with a leg of 45mm. As per specification this fillet weld would require PWHT.
I would like to know if the requirement of PWHT can be avoided, as they have already qualified a CJP WPS without PWHT, that would cover up to 40mm (over 40mm would require PWHT), and this would cover all fillet welds.