Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

PQR qualification confusion

Status
Not open for further replies.

gkvengat

Mechanical
Oct 19, 2013
34
Dear frienda,
I have 7.6mm,10.3mm,11.6 and 16 mm thickness of three different thickness in which thichness i have qualify the PQR to cover the all three thickness range ...i have the impact test requirement also.....
 
Replies continue below

Recommended for you

gkvengat,
Even you have not told us the applicable code, the 10.3 mm could qualify for such a variety of thicknesses to the majority of codes
regards
wegm
 
wegm,
In accordance with ASME IX QW 403.6 the minimum thickness qualified is 10.3 mm so how does that qualify a thickness of 7.6 mm ?
Regards,
DD
 
Per B31.3, the 10.3 mm coupon qualifies for all your thickness [ T/2 to T + 1/4"). Per ASME VIII the 10.3 mm plate qualification qualifies the range of 10.3 mm to 20.6 mm per ASME IX.
 