Aug 10, 2017 #1 mulz Mechanical Jul 15, 2015 18 0 0 SA Dear, What is the pre-heating temperature in the latest edition of asme b31.3 coz we are dealing with welding of piping whose diameter is 16'',cs, sch.80.. Thanks mulz
Dear, What is the pre-heating temperature in the latest edition of asme b31.3 coz we are dealing with welding of piping whose diameter is 16'',cs, sch.80.. Thanks mulz
Aug 10, 2017 4 #2 DekDee Petroleum Mar 12, 2012 1,275 0 36 PH If you are working to the latest edition of B31.3 then you had better purchase a copy. Upvote 0 Downvote
Aug 10, 2017 #3 XL83NL Mechanical Mar 3, 2011 3,043 0 36 NL DD's reply is the best youll get to your question. Upvote 0 Downvote
Aug 10, 2017 #4 david339933 Industrial Jun 15, 2011 1,204 0 0 CA When you do get a copy, check out Table 330.1.1 Upvote 0 Downvote