marcolino21576
Materials
Dear All,
I have one question. Our welder is carrying out a qualification of a new WPS, by welding a cast coupon in duplex 2205 with duplex 2209. The welding activities shall be distributed during 5 days.
To reduce to minimum the presence of humidity on the weld, the welder shall lightly pass the flame of a burner on the weld surface. This is going to happen each day, before starting welding activities.
Should this "drying" activity be considered formally as preheating and (= should the temperature of the weld joing be registered on the WR?)
Thank you for your help
MC
I have one question. Our welder is carrying out a qualification of a new WPS, by welding a cast coupon in duplex 2205 with duplex 2209. The welding activities shall be distributed during 5 days.
To reduce to minimum the presence of humidity on the weld, the welder shall lightly pass the flame of a burner on the weld surface. This is going to happen each day, before starting welding activities.
Should this "drying" activity be considered formally as preheating and (= should the temperature of the weld joing be registered on the WR?)
Thank you for your help
MC