vinothsvk
Mechanical
- May 19, 2016
- 27
Dear All,
As per ASME SEC VIII DIV-I Table UCS 56-1 General Notes (b)(2), For weld joints over 32mm nominal thickness to 38mm nominal thickness unless preheat is applied at a minimum temperature of 95 degree Celsius during welding.This preheat is not be applied to SA841 grades A and B provided that the carbon content and carbon equivalent(CE) for plate material, by heat analysis do not exceed 0.14% and 0.40%
Is this statement can be applied to all material (for example SA516 Grade 55,60,65 and 70)?
As per ASME SEC VIII DIV-I Table UCS 56-1 General Notes (b)(2), For weld joints over 32mm nominal thickness to 38mm nominal thickness unless preheat is applied at a minimum temperature of 95 degree Celsius during welding.This preheat is not be applied to SA841 grades A and B provided that the carbon content and carbon equivalent(CE) for plate material, by heat analysis do not exceed 0.14% and 0.40%
Is this statement can be applied to all material (for example SA516 Grade 55,60,65 and 70)?