6
I prepared wps according to pqr, preheat temperature is not stated in pqr, so I write it in wps NA, but the Client need to add it in the WPS
WHAT can i do?
wps and pqr according to asmi ix
weather temperature is about 31°C to 38°C
 
Replies continue below

Recommended for you


Decrease in Pre heat is essential variable so you should note temperature value.
 
can I state it ambient temperature
 
If you did not apply preheat, use the ambient temperature condition on the PQR for preheat prior to welding.
 