Greetings All,
I read in a previous thread that CSA Z662 requires pressure testing after backfilling. However, I read this standard but I didn’t find this requirement. Can someone please point me out to this requirement in this code? Which clause? Also, are there other standards that mandate the same thing. In my company we apply pressure testing while joints are exposed for underground nonmetallic piping. I want to share this practice here but I desperately needs the exact quotation.
Thanks
I read in a previous thread that CSA Z662 requires pressure testing after backfilling. However, I read this standard but I didn’t find this requirement. Can someone please point me out to this requirement in this code? Which clause? Also, are there other standards that mandate the same thing. In my company we apply pressure testing while joints are exposed for underground nonmetallic piping. I want to share this practice here but I desperately needs the exact quotation.