Need your help.i got datasheet from client need to design Division 2 vessel.
ID : 2320
length shell : 6245
Internal pressure : 165 Bars
External Pressure : FV
Temperature : 70/70
Head Type : Body flange (Top),Hemispherical Head (Bottom)
material head and shell : SA 516 GR.70
body flange material " SA.350 LF.2 CL.1
When i come out in PV elite. requirement thickness body flange is 500 mm thickness. have other way how to reduced thickness of body flange?
Thank You so much if can help me to solve this problem
ID : 2320
length shell : 6245
Internal pressure : 165 Bars
External Pressure : FV
Temperature : 70/70
Head Type : Body flange (Top),Hemispherical Head (Bottom)
material head and shell : SA 516 GR.70
body flange material " SA.350 LF.2 CL.1
When i come out in PV elite. requirement thickness body flange is 500 mm thickness. have other way how to reduced thickness of body flange?
Thank You so much if can help me to solve this problem