For the fatigue assessment of a welded component, an SN curve is given that is generally a line of best fit through data of stress (S) against the number of cycles to failure (N).
What is the probability of 2 or more welded components, subject to the same stress, failing at the same time or failing within a certain number of cycles of each other?

corus
 
Replies continue below

Recommended for you

Let's call the lowest failure n1 cycles, and the second n2

We can fairly confidently say that p(n1=n2)=~0 if n1>1000


You could do a Weibull analysis.


for a hideously complicated explanation. Also shows a worked example of how you do a weibull analysis in practice

Failing that, an ad hoc approach is to say that on average the mean life is .5(n1+n2), and on average 1/3 of the population will fail before n1, 1/3 between n1 and n2, and one third above n2. The proper analysis of this actually gives 29% below n1, and 29% above n2, and obviously 42% between them.


describes how to estimate standard deviations from small sample sizes.

Cheers

Greg Locock
 