Hi all, some advice please!! Thank you in advance!
A few weeks ago i cut 8mm stainless on our 2.2 kw bystronic, using default settings, and had a brilliant cut - no burrs or anything! I am now trying to cut some again and the cut edge is still brilliant but there are massive (approx 3-5mm long) jagged burs coming of the bottom edge! I have tried everything to remove them with no luck, e.g. cleaned the lens, checked alignment, altered the cut speed, gas, focal point, etc. If anyone can help it would be much appreciated.
I put a sheet of 5mm stainless, and 6mm stainless in and that cut perfectly too (no burrs), but its not cutting the 8mm! Also, the 8mm is the same sheet which i previously cut very well, so it can't be the material!!
Thanks all,
sjclaser.
A few weeks ago i cut 8mm stainless on our 2.2 kw bystronic, using default settings, and had a brilliant cut - no burrs or anything! I am now trying to cut some again and the cut edge is still brilliant but there are massive (approx 3-5mm long) jagged burs coming of the bottom edge! I have tried everything to remove them with no luck, e.g. cleaned the lens, checked alignment, altered the cut speed, gas, focal point, etc. If anyone can help it would be much appreciated.
I put a sheet of 5mm stainless, and 6mm stainless in and that cut perfectly too (no burrs), but its not cutting the 8mm! Also, the 8mm is the same sheet which i previously cut very well, so it can't be the material!!
Thanks all,
sjclaser.