bearingsteel
Materials
- Jun 21, 2012
- 23
What parameters of heat treatment should i use for steel SH15G-v and SH15SG-v if i want to reaveal carbide bands? I use the same heat treatment for both steel marks but it's not always good , because sometimes instead of white bands i get them black and can't figure out how to proper analyse them.