has anyone experienced problems with Gylon (restructured TFE) gaskets?
 
Replies continue below

Recommended for you

What particular problems are you concerned about? It's simply reinforced teflon with all the strengths (chemical resistance) and problems (creep) of that material.
 
chemical--going into sulfuric alkylation service.
 