Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Product Analysis - API 5CT for Casing and Tubing

Status
Not open for further replies.

Lijohn

Mechanical
May 9, 2018
2
As per API 5CT, clause 10.3.2, two tubular products from each heat used shall be analysed for product analysis. However, we observed that some of the reputed pipe manufacturers are producing a single pipe under one heat. Therefore, manufacturer confirmed that only one product analysis is possible for that particular heat as there is only one pipe produced under that heat.

Please advise whether single product analysis is acceptable or that single pipe is to be rejected as it is not complying to the requirements of clause 10.3.2 of API 5CT.
 