Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Production Welding Before WPS is Qualified - AS/NZS 1554.1:2014

Status
Not open for further replies.
Is it normal for a welding code to allow production welding to start BEFORE a PQR is run? Once the procedure is qualified then it covers the welds already welded, is that a normal provision in a code for PQR & WPS's? It is in AS/NZS 1554.1 - 2014 with no time limit on how long you can run production welds before the WPS must be qualified. Yet in another location it says you must qualify prior to production welding.

Fabricators will tend to take advantage if there are anomalies. What is the norm here?
 
Not that familiar with AS/NZS standards but they are generally pretty good. The presumption is always that a PQR would be done before production welding. They are not to be applied retroactively. Makes no sense to do so.


A Great Place For Engineers to Help Engineers

Follow me there.....
 
Thanks Ron

Perhaps take a look at 4.2 (c) & 4.7.3.

There is no time limit on these provisions. Should we make it the very last weld on the project? Some would try I am sure.
 