I have encounter premature prop shaft failure (bearing failure on spider)initial accessment suggested that the big angle of deflection (17degrees_shaft max of 23 degrees)had caused the seal of the needle bearing to fail 1st and as a result debries enters and bearing siezed. I am aware that by reducing the angle or deflection, reducing the speed the failure can be averted and also the bearing is likely to be the component to fail 1st in such cases. Is there anyone out there who had experiences in such problem and manage to find a solution by doing something to the bearing?