Inchtain
Petroleum
- Feb 21, 2021
- 151
Good morning,
Our plan is to perform an external/on-stream inspection for a Propane Sphere Storage Tank including visual and UT thickness measurement only to assess its existing situation.
Can anyone provide me with a typical grid as CMLs (Corrosion Monitoring Locations) used to measure the thickness? and I would also appreciate any advice concerning the subject.
Could you be kind enough to inform me about the critical points to focus during our inspection?
Thank you very much.
Our plan is to perform an external/on-stream inspection for a Propane Sphere Storage Tank including visual and UT thickness measurement only to assess its existing situation.
Can anyone provide me with a typical grid as CMLs (Corrosion Monitoring Locations) used to measure the thickness? and I would also appreciate any advice concerning the subject.
Could you be kind enough to inform me about the critical points to focus during our inspection?
Thank you very much.