A PRV is installed at our site on Liquid Ammonia Service with operating temperature of 90F and Operating Pressure of 300 Psig. CDTP of PRV as mentioned on nameplate is 600 Psig and same is used during its calibration in shop.
Icing was reported on PRV body at disc area in past month (picture attached). This PRV was brought to our shop facility for calibration and pressure testing. No issue was found in Pressure and Leakage test in “as found condition”. PRV calibration was also found Okay and we installed it back.
Same issue of icing was reported after a couple of days of its installation. PRV was again brought to shop facility for pressure and leakage tests and no issue was found. Inspection of PRV internals was also carried out this time and no anomaly was found.
In the light of your experience, what do you people think should be the probable causes of this recurring issue?
Thanks,
JZ59
Icing was reported on PRV body at disc area in past month (picture attached). This PRV was brought to our shop facility for calibration and pressure testing. No issue was found in Pressure and Leakage test in “as found condition”. PRV calibration was also found Okay and we installed it back.
Same issue of icing was reported after a couple of days of its installation. PRV was again brought to shop facility for pressure and leakage tests and no issue was found. Inspection of PRV internals was also carried out this time and no anomaly was found.
In the light of your experience, what do you people think should be the probable causes of this recurring issue?
Thanks,
JZ59