Well , one question came in my mind while discussion with some inspection engineers , that , In a butt welding , ( Joint is single V and diameter is 43" ) we are doing the GTAW in root and hot pass , so after completion of Weld , Is we need to do PT / MPI from root side ? We are doing PT / MPI from face side ( top side not inside )
Is any code reference for the same if required or if not required then there is any code reference ?
Kindly help us ..
Regards
nAVIN
Well , one question came in my mind while discussion with some inspection engineers , that , In a butt welding , ( Joint is single V and diameter is 43" ) we are doing the GTAW in root and hot pass , so after completion of Weld , Is we need to do PT / MPI from root side ? We are doing PT / MPI from face side ( top side not inside )
Is any code reference for the same if required or if not required then there is any code reference ?
Kindly help us ..
Regards