Dear all, in reference with the above subject, please do note that the NDT guy can be right by requesting PT on a root weld.
It is true ASME doesnt require such, but it is equally true that additional standards such as NACE MR0175 or NACE MR0103, referring to NACE SP0472 welding procedure may require this on all root welding, specially when doing WPQ/PQR.
Upon discussion and negotiation with your customer you may or may not override some or all of these requirements depending on the criticallity of the service you are handling and the expected media (HIC,SCC,SCCA...)
Best regards.
Dear all, in reference with the above subject, please do note that the NDT guy can be right by requesting PT on a root weld.
It is true ASME doesnt require such, but it is equally true that additional standards such as NACE MR0175 or NACE MR0103, referring to NACE SP0472 welding procedure may require this on all root welding, specially when doing WPQ/PQR.
Upon discussion and negotiation with your customer you may or may not override some or all of these requirements depending on the criticallity of the service you are handling and the expected media (HIC,SCC,SCCA...)
Best regards.