weldstan
Materials
- Jun 24, 2011
- 2,788
An NCR must be a true nonconformance and mmust be specified as to what part of the contract work is noncompliant. In your statement, the PT requirement proposed by the NDE guy is not a part of the contract. If the QA/QC department dictates how the work in the shop is to be performed, so be it. However the "NDE guy" is not the QA/QC department and the department can over rule the "NDE guy's" position as well as can management. Your hypothetical arguement is not really relavent to any of the Code shops that I have been involved with in 40+ years or the Qualty plans that I have co-written for a number of major EPC companies.
As the responsible Engineer, I have required root pass PT in specific instances and have specified and written the PT procedure to be followed.