SandraB
Materials
- Nov 30, 2020
- 3
Hello everyone! I am interesting in all info about PTFE streamline liners. Maybe someone could give some advise on stretching this liner onto the mandrel? What are the main causes of delamination when using PTFE liner? Pros and cons of this liner? Thank you!