Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Puddle (Arc Spot) Welds 1

Status
Not open for further replies.

MacGruber22

Structural
Jan 30, 2014
802
Is there an interaction equation for shear and tension on these welds? I don't see anything in the AWS D1.3

I was thinking maybe a single spot weld may not be permitted to resist combined loading, and the answer is to have more welds.

The application is diaphragm and uplift loads on metal roof deck.
 
Replies continue below

Recommended for you

Excellent, Ron.

I am surprised they even bothered with the nonlinear regression based on the scatter.
 