Gents,
Can pullout strength (e.g. of an insert or bolt)of composite be determined by analysis??
 
Replies continue below

Recommended for you

Yes, but pull-thru strength is a very complicated mix of failure modes. Have tried to correlate several analyses with data without much success, unless one is very conservative with assumptions.
 
Normal load can be applied to surface and then check material permissible stresses and strains. Do you have glass fibers or carbon fibers?
 
ameyard,
the fibres are carbon fibre in fabric and UD form. Could you be more specific with regards to the material permissible stresses and strains

 