Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

PVC & UL 94 flammability

Status
Not open for further replies.

boldfish

Mechanical
Jan 29, 2003
101
Does all PVC meet V0 requirements as set forth by UL 94 due to its self extinguishing properties or does it depend upon formulation/usage e.g. extrusion, molded, etc.? I know that additives are often used to make a thermoplastic meet the requirement but I'm not sure if the PVC that is V0 has these additives or not.

How does one go about ensuring this requirement is met?

 
Replies continue below

Recommended for you

Ask your raw material supplier or moulder or parts supplier.

You could have a part tested.

PVC is normally a compound that contains additives to improve it's mould ability. These could be detrimental to pure PVCs natural inclination to be flame retardant. I am not sure if PVC needs the help of additives to get a V0 rating.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor