Dear Experts,
Base material is SA516Gr70 and cladding is Incoel 625. H2S service.
1. My understanding is that it is not required PWHT due to H2S service for the cladding vessel because H2S is not contact to the base material of CS. Any different opinions with my view?
2. Cladding vessel after PWHT may cause layered blistering due to the different thermal expansion rate betwween base material and the cladding. Is it possible to make sure 100% no layered blistering after PWHT for cladding vessel?
Thanks.