mechengineer
Mechanical
- Apr 19, 2001
- 268
Hi,
For SA-213 T9 (P-No.5B, Group No.1) tubes, it is an 9Cr–1Mo steel. According to ASME Ⅷ-1 UCS-56 Table UCS-56-4, the tube joint needs to undergo PWHT at the minimum heat treatment temperature of 675℃.
The material of tubesheet is SA-266 Gr.3 (P-No.1, Group No.2). According to ASME Ⅷ-1 UCS-56 Table UCS-56-1, the minimum PWHT of the tubesheet is 595℃. At the same time, the heat treatment process of tubesheet will adopt quenched and tempered, with the optimal tempered temperature is 620℃~630℃.
If PWHT is carried out according to the SA-213 T9, will it damage the properties of SA-266 Gr.3 material?
Regards,
For SA-213 T9 (P-No.5B, Group No.1) tubes, it is an 9Cr–1Mo steel. According to ASME Ⅷ-1 UCS-56 Table UCS-56-4, the tube joint needs to undergo PWHT at the minimum heat treatment temperature of 675℃.
The material of tubesheet is SA-266 Gr.3 (P-No.1, Group No.2). According to ASME Ⅷ-1 UCS-56 Table UCS-56-1, the minimum PWHT of the tubesheet is 595℃. At the same time, the heat treatment process of tubesheet will adopt quenched and tempered, with the optimal tempered temperature is 620℃~630℃.
If PWHT is carried out according to the SA-213 T9, will it damage the properties of SA-266 Gr.3 material?
Regards,