Dear All,
In the asme 31.3 table 331.1.3 exemption to mandatory PWHT. Mentioned that For P5A, group no.1- less than or equal to 16mm thickness -groove-Mandatory pre-heat is applied (see attached file for details) is exempted to PWHT.
Our project:
We have tie-in activity the existing pipe thickness is 20mm and the material specification is 10CrMo9.10. The new material to be connected is 10mm thickness and 321H grade. Tapering to be done on existing pipe to match the new piping, since the joint thickness is below 16mm, is it applicable the mentioned table?
Thanks in advance.
In the asme 31.3 table 331.1.3 exemption to mandatory PWHT. Mentioned that For P5A, group no.1- less than or equal to 16mm thickness -groove-Mandatory pre-heat is applied (see attached file for details) is exempted to PWHT.
Our project:
We have tie-in activity the existing pipe thickness is 20mm and the material specification is 10CrMo9.10. The new material to be connected is 10mm thickness and 321H grade. Tapering to be done on existing pipe to match the new piping, since the joint thickness is below 16mm, is it applicable the mentioned table?
Thanks in advance.