Guys i need your help to answer the below

We have cs-0.5mo pipe 16mm thickness with heavy external corrosion
I recommended to use 8018-B2 electrod for weld build up with PWHT at 620c


Is the electrod right and do i need higher PWHT temp
 
Replies continue below

Recommended for you

It is not necessarily wrong but why not use a matching E7018-A1 filler, a 200F preheat and no PWHT?
 
I had wps for p3 to p4 i had to use it.