Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Quolifying thickness reducetion for forming head of pressure vessel in fabrication

Status
Not open for further replies.

mechengineer

Mechanical
Apr 19, 2001
267
Hi QC experts,
I have a vendor, the nominal dished head thickness is 14 mm, after forming 7 mm, the stress calculation thickness required is 6 mm. It is ok in deign/stress calculation. But I don't believe it is a good/qualified product with reduced a half of the nominal thickness after forming, some where thickness reduced from 14 mm to 7 mm. Any regulations from code, user's specifications and fabrication experience for qualifying the forming head thickness reduction?
Thanks
 
Replies continue below

Recommended for you

Depends on the required pressure. Someone needs to do a stress analysis using the actual thicknesses.
 
You don't give a lot of info, but I would check out UCS-79 (d)(2)(d)
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor