Hi Experts,
Would like to seek your opinion on the rail crack (see attached). Please advise.
1. Is that consider a beach mark around the circular patch? To me, it seem more like an oxidation rather than beach mark.
2. Consider thermite welding was performed to this rail 7 years ago, how will it affect the surrounding material? I noticed inclusion in the middle of the rail. Such failure could be due to the process but I am surprised it actually survived for 7 years w/o failing.
3. What are some of the possible defects that I have missed out? I saw ratchet marks.
Thanks all.
Would like to seek your opinion on the rail crack (see attached). Please advise.
1. Is that consider a beach mark around the circular patch? To me, it seem more like an oxidation rather than beach mark.
2. Consider thermite welding was performed to this rail 7 years ago, how will it affect the surrounding material? I noticed inclusion in the middle of the rail. Such failure could be due to the process but I am surprised it actually survived for 7 years w/o failing.
3. What are some of the possible defects that I have missed out? I saw ratchet marks.
Thanks all.