I am designing a UPRR underpass, multi-tracks, the superstructure is steel plate girder with steel deck, located in Arizona.
I have some question on the ASTM.
I designed the steel girder using 50ksi steel, but i am having hard time with what kind of ASTM steel to be used for this bridge.
I am very confused which one to be used between ASTM A709 GRADE50 no wearthering and no-FCM, and ASTM A572 GRADE50.
Per AREMA code, page 15-1-10, table 15-1-3, the ASTM A709 GRADE 50 is equvalent to ASTM A572 GRADE 50.
My main concern is the unit price per Ibs. According to the fabricators which i called, ASTM A709 steel is more expensive than ASTM A572 steel. If the two ASTM are equivalent per AREMA, why we should even think of using ASTM A572, because it is cheaper?
My 30% estimate is based on ASTM A572. I have to increase the estimate cost by minimum 25% if i have to use ASTM A709 for 60% submittal.
Please help!!!
I have some question on the ASTM.
I designed the steel girder using 50ksi steel, but i am having hard time with what kind of ASTM steel to be used for this bridge.
I am very confused which one to be used between ASTM A709 GRADE50 no wearthering and no-FCM, and ASTM A572 GRADE50.
Per AREMA code, page 15-1-10, table 15-1-3, the ASTM A709 GRADE 50 is equvalent to ASTM A572 GRADE 50.
My main concern is the unit price per Ibs. According to the fabricators which i called, ASTM A709 steel is more expensive than ASTM A572 steel. If the two ASTM are equivalent per AREMA, why we should even think of using ASTM A572, because it is cheaper?
My 30% estimate is based on ASTM A572. I have to increase the estimate cost by minimum 25% if i have to use ASTM A709 for 60% submittal.
Please help!!!