Maurijr
Petroleum
- Mar 1, 2014
- 7
Hello friends, please help me
If i Have to qualify a procedure whit thickness 10 mm. Smaw with impact test
Wich is mandatory to define range thickness?
Asme b31.3 tab. 323.3.1 A-5 or Asme Ix 403.6 and 451
Minimum qualified it's 10mm, 403.6 asme IX. Ok, but maximun it's T+6mm like Asme b31.3 tab. 323.3.1 A-5 or 2T like QW451????
Thanks a lot!!
If i Have to qualify a procedure whit thickness 10 mm. Smaw with impact test
Wich is mandatory to define range thickness?
Asme b31.3 tab. 323.3.1 A-5 or Asme Ix 403.6 and 451
Minimum qualified it's 10mm, 403.6 asme IX. Ok, but maximun it's T+6mm like Asme b31.3 tab. 323.3.1 A-5 or 2T like QW451????