We had purchased flanges(SA182 F316L) from a vendor, while reviewing their test certificate i came across the 'raw material used' column which says SS Round bar.
ASME Section VIII Div.1 UG-14 says 'Except for flanges of all types, hollow cylindrically shaped parts may be machined from rods & bars. Similarly Section II-A SA182 Para 6.4.1 & Section II-A SA961 para 6.1.1 says Flanges of any type, elbows, return bend shall not be machined directly from rods & bars.
Since the flange is for manufacturing a pressure vessel with 'U' stamp, whether we have to replace it.
Can anyone please advice whether my interpretation is right?
Thanks & Regards
M.V.Silambarasan
+919591507348
We had purchased flanges(SA182 F316L) from a vendor, while reviewing their test certificate i came across the 'raw material used' column which says SS Round bar.
ASME Section VIII Div.1 UG-14 says 'Except for flanges of all types, hollow cylindrically shaped parts may be machined from rods & bars. Similarly Section II-A SA182 Para 6.4.1 & Section II-A SA961 para 6.1.1 says Flanges of any type, elbows, return bend shall not be machined directly from rods & bars.
Since the flange is for manufacturing a pressure vessel with 'U' stamp, whether we have to replace it.
Can anyone please advice whether my interpretation is right?
Thanks & Regards
M.V.Silambarasan