Cisnerjo1973
Aerospace
- Jul 6, 2016
- 19
Hello,
I have a question why the phenolic prepregs get a different cure cycle than the epoxy ones. Customer request a dwell or stabilization step for 30 minutes for the phenolic prepreg at temperature of 175°F to 185°F. After those 30 minutes the temperature goes up again up to 260°F for 90 minutes cure.
How is that process call and why is performed or whats the main purpose of it? I mean about the 30 minutes at 175°F to 185°F.
Thanks for your valuable support!
I have a question why the phenolic prepregs get a different cure cycle than the epoxy ones. Customer request a dwell or stabilization step for 30 minutes for the phenolic prepreg at temperature of 175°F to 185°F. After those 30 minutes the temperature goes up again up to 260°F for 90 minutes cure.
How is that process call and why is performed or whats the main purpose of it? I mean about the 30 minutes at 175°F to 185°F.
Thanks for your valuable support!