Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Recommendation for strong clear film-grade material 1

Status
Not open for further replies.

walkingcube

Mechanical
Aug 23, 2010
8
Hello,

I'm currently looking into a material that can be blown into strong, (almost optically) clear films.

We're currently doing some stretch blow moulding for a client on transparent bag-like food containers with very thin walls (.0025" in thickness) and have been experimenting with some film-grade PA12 (ex: Grilamid L25) with some success. However, we're looking something that with a higher tensile strength.

Does anyone have any suggestion as to what I should look into?


Thanks!


 
Replies continue below

Recommended for you

PA12 will take some beating.

PA11 might be a little better.

Polysulphone might be worth a look.

Most data I have is for injection moulding and material rankings do change due to differing effects from being stretched in the film blowing process.

Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
for site rules
 
If you really want to thank somebody on this forum, click the link with the little pink star next to it.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor