Hello,

I have found some datasheets of Kokam Li-Pol batteries. And there were information, about recoverable capacity after storage:

The recoverable capacity of them is >90% (after 6 months storage at temperature 23°C)

My question is if that is true?
In my opinion is 10% permanent loss of capacity too much after six month of storage.

Does anybody have some experiences with Li-Pol batteris and with their loss of capacity during storage?

Thank You
 
Replies continue below

Recommended for you

And I thought they should be better.
So it looks like that they are not.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor